Energy Environ. Sci., 2024, 17,1975-1983
DOI: 10.1039/D3EE04515C, Paper
DOI: 10.1039/D3EE04515C, Paper
Huijun Yang, Yang Yang, Wuhai Yang, Gang Wu, Ruijie Zhu
We correlate the Zn plating/stripping cyclability with the kinetics of hydrogen evolution. The pronounced hydrogen evolution kinetics and asymmetric Zn plating/stripping kinetics explain the poor Zn reversibility at low current density.
The content of this RSS Feed (c) The Royal Society of Chemistry
We correlate the Zn plating/stripping cyclability with the kinetics of hydrogen evolution. The pronounced hydrogen evolution kinetics and asymmetric Zn plating/stripping kinetics explain the poor Zn reversibility at low current density.